三维互穿结构SiC晶须骨架增强镁基复合材料制备及其力学性能
谷瑞成, 张健, 张明阳, 刘艳艳, 王绍钢, 焦大, 刘增乾, 张哲峰

Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties
GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng
图6 经1200℃预氧化处理得到的以纯Mg和AZ91D镁合金为基体的SiCw/Mg复合材料的J积分和相对应的应力强度因子(KJ)随 裂纹扩展长度(Δa)的变化曲线(以AZ91D镁合金为基体的复合材料的断裂韧性水平以虚线表示)
Fig.6 Curves of J-integral (a) and K-based fracture toughness (KJ) (b) with crack extension (Δa) measured by in situ SEM for the SiCw/Mg composites with pure Mg and AZ91D Mg alloy as the matrices corresponding to pre-oxidation temperature of SiCw scaffolds of 1200oC (The dashed lines indicate the fracture toughness values of the composite with AZ91D Mg alloy as the matrix)