Ti及钛合金表面改性在生物医用领域的研究进展 |
| 崔振铎, 朱家民, 姜辉, 吴水林, 朱胜利 |
|
Research Progress of the Surface Modification of Titanium and Titanium Alloys for Biomedical Application |
| CUI Zhenduo, ZHU Jiamin, JIANG Hui, WU Shuilin, ZHU Shengli |
| 图3 喷砂、酸蚀及其组合,3D打印及激光表面纹理化示意图 |
| Fig.3 Schematics of sandblasting, acid etching, and their combination (a), 3D printing (b), and laser surface texturing (c) |
|