Ti及钛合金表面改性在生物医用领域的研究进展 |
| 崔振铎, 朱家民, 姜辉, 吴水林, 朱胜利 |
|
Research Progress of the Surface Modification of Titanium and Titanium Alloys for Biomedical Application |
| CUI Zhenduo, ZHU Jiamin, JIANG Hui, WU Shuilin, ZHU Shengli |
| 图2 放电等离子烧结制备Ti-Mg合金和钛合金激光表面改性示意图 |
| Fig.2 Schematics of the preparation of Ti-Mg alloy by spark plasma sintering (a) and laser surface modification of Ti alloy (b) |
|