基于二次枝晶间距变化特征的连铸方坯CET位置判断新方法 |
||||||||||||||||||||
| 郭东伟, 郭坤辉, 张福利, 张飞, 曹江海, 侯自兵 | ||||||||||||||||||||
|
A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing |
||||||||||||||||||||
| GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing | ||||||||||||||||||||
| 表3 No.1铸坯右侧表面中心测温结果与温度场数值模拟结果对比 |
||||||||||||||||||||
| Table 3 Comparison of temperature measurement results and numerical simulation results of temperature field at the center of right surface of billet No.1 |
||||||||||||||||||||
|
||||||||||||||||||||