表2 温度场计算过程中各部分参数及计算公式[18~20]
|
Table 2 Parameters and relevant computational formulas at different sections in the calculation of temperature field[18-20]
|
|
| Section | Length | Water amount | Boundary condition | Computational formula |
|---|
| m | m3·h-1 | | | | | No.1 | No.2 | | | | Mold | 0.9 | 114 | 114 | qm | | | Foot roller section | 0.5 | 4.16 | 5.19 | qf = hf(Tb - Tf) | hf = 153.6(w / 60)0.351 | | First section of secondary cooling zone | 2.7 | 6.69 | 8.24 | qk = hk(Tb - Tw) | hk = 160 + 8.35w0.851 | | Second section of secondary cooling zone | 2.9 | 2.08 | 2.48 | qk = hk(Tb - Tw) | hk = 200 + 10.44w0.851 | | Third section of secondary cooling zone | 3.5 | 1.63 | 2.04 | qk = hk(Tb - Tw) | hk = 200 + 10.44w0.851 | | Air cooling zone | 5.4 | - | - | qa = ɛσ(Tb4 - Ta4) | ε = 0.8 |
|
|
|