基于二次枝晶间距变化特征的连铸方坯CET位置判断新方法 |
| 郭东伟, 郭坤辉, 张福利, 张飞, 曹江海, 侯自兵 |
|
A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing |
| GUO Dongwei, GUO Kunhui, ZHANG Fuli, ZHANG Fei, CAO Jianghai, HOU Zibing |
| 图2 连铸坯试样横断面二次枝晶间距(SDAS)测量位置 |
| Fig.2 Schematic of measurement position of secondary dendrite arm spacing (SDAS) in cross section of selected continuous casting billets |
|