Zr61Cu25Al12Ti2 和Zr52.5Cu17.9Ni14.6Al10Ti5 块体非晶合金过冷液相区的塑性流变行为
刘帅帅, 侯超楠, 王恩刚, 贾鹏

Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region
LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng
图10 非晶合金过冷液相区Newtonian黏度和温度的变化关系
Fig.10 Dependence of viscosity in the temperature in the supercooled liquid region of amorphous alloys (The fitting curves are deduced from Eq.(3). ηVFT—pre-exponential factor, D*—fragility parameter, T0—VFT temperature)