Zr61Cu25Al12Ti2 和Zr52.5Cu17.9Ni14.6Al10Ti5 块体非晶合金过冷液相区的塑性流变行为
刘帅帅, 侯超楠, 王恩刚, 贾鹏

Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region
LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng
图6 ZT1和Vit105非晶合金应变速率与流变应力之间的关系
Fig.6 Variation relationships of the flow stress with the applied strain rate in ZT1 (a) and Vit105 (b) amorphous alloys at different temperatures (The solid lines are deduced from Eq.(1))