Zr61Cu25Al12Ti2 和Zr52.5Cu17.9Ni14.6Al10Ti5 块体非晶合金过冷液相区的塑性流变行为
刘帅帅, 侯超楠, 王恩刚, 贾鹏

Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region
LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng
图4 不同应变速率时,663 K下ZT1和683 K下Vit105非晶合金的真应力-真应变曲线
Fig.4 True stress-true strain curves of ZT1 (at 663 K) (a) and Vit105 (at 683 K) (b) amorphous alloys with different strain rates