Zr61Cu25Al12Ti2 和Zr52.5Cu17.9Ni14.6Al10Ti5 块体非晶合金过冷液相区的塑性流变行为
刘帅帅, 侯超楠, 王恩刚, 贾鹏

Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region
LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng
图3 应变速率为1 × 10-3 s-1时,ZT1合金在688和693 K以及Vit105合金在723 K热塑性变形后的XRD谱
Fig.3 XRD spectra of ZT1 amorphous alloy at 688 and 693 K, and Vit105 amorphous alloy at 723 K after thermoplastic compressive deformation with constant strain rate of 1 × 10-3 s-1