Zr61Cu25Al12Ti2 和Zr52.5Cu17.9Ni14.6Al10Ti5 块体非晶合金过冷液相区的塑性流变行为
刘帅帅, 侯超楠, 王恩刚, 贾鹏

Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region
LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng
图2 应变速率为1 × 10-3 s-1、不同温度下ZT1和Vit105非晶合金的真应力-真应变曲线
Fig.2 True stress-strain curves of ZT1 (a) and Vit105 (b) amorphous alloys at different temperatures with constant strain rate of 1 × 10-3 s-1