Zr61Cu25Al12Ti2 和Zr52.5Cu17.9Ni14.6Al10Ti5 块体非晶合金过冷液相区的塑性流变行为
刘帅帅, 侯超楠, 王恩刚, 贾鹏

Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region
LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng
图1 Zr61Cu25Al12Ti2 (ZT1)和Zr52.5Cu17.9Ni14.6Al10Ti5 (Vit-105)非晶合金的XRD谱和DSC曲线
Fig.1 XRD spectra (a) and DSC curves (b) of Zr61Cu25Al12Ti2 (ZT1) and Zr52.5Cu17.9Ni14.6Al10Ti5 (Vit105) amorphous alloys (Tg and Tx are the glass transition temperature and crystallization temperature, respectively)