Fe76Ga5Ge5B6P7Cu1 合金的非等温晶化动力学 |
| 郭璐, 朱乾科, 陈哲, 张克维, 姜勇 |
|
Non-Isothermal Crystallization Kinetics of Fe76Ga5Ge5B6P7Cu1 Alloy |
| GUO Lu, ZHU Qianke, CHEN Zhe, ZHANG Kewei, JIANG Yong |
| 图6 升温速率10 K/min、退火温度400℃和升温速率100 K/min、退火温度425℃时Fe76Ga5Ge5B6P7Cu1合金退火后的TEM像、SAED花样和晶粒尺寸分布及晶化示意图 |
| Fig.6 TEM images, SAED patterns, and grain size distributions of Fe76Ga5Ge5B6P7Cu1 ribbons annealed at 400oC with heating rate of 10 K/min (a) and 425oC with heating rate of 100 K/min (b), and schematic of the crystallization of Fe76Ga5Ge5B6P7Cu1 alloys (c) |
|