热挤压Zn-2Cu-0.5Zr合金的力学性能与降解行为 |
| 沈岗, 张文泰, 周超, 纪焕中, 罗恩, 张海军, 万国江 |
|
Mechanical Properties and Degradation Behavior of Hot-Extruded Zn-2Cu-0.5Zr Alloy |
| SHEN Gang, ZHANG Wentai, ZHOU Chao, JI Huanzhong, LUO En, ZHANG Haijun, WAN Guojiang |
| 图11 热挤压Zn-2Cu-0.5Zr合金性能改善机制示意图 |
| Fig.11 Schematic of the improvement mechanisms for the enhanced mechanical properties and degradation behavior of hot-extruded Zn-2Cu-0.5Zr alloy |
|