预变形和双级时效对Fe-30Mn-11Al-1.2C奥氏体低密度钢显微组织和力学性能的影响 |
| 任平, 陈兴品, 王存宇, 俞峰, 曹文全 |
|
Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel |
| REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan |
| 图9 κ′碳化物(110)晶面原子排布和反相畴界示意图 |
| Fig.9 Schematics of the atomic arrangement of (110) plane of κ′ carbide (a) and the antiphase boundary (APB) (b) |
|