预变形和双级时效对Fe-30Mn-11Al-1.2C奥氏体低密度钢显微组织和力学性能的影响 |
| 任平, 陈兴品, 王存宇, 俞峰, 曹文全 |
|
Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel |
| REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan |
| 图6 CR + A1态Fe-30Mn-11Al-1.2C钢的TEM明场像、κ′碳化物TEM暗场像及κ′碳化物SAED花样 |
| Fig.6 Bright field TEM image of sample CR + A1 (a), dark field TEM image of κ′-carbide (b), and SAED pattern of κ′-carbide along [001] γzone axis (c) |
|