蠕变时效对欠时效7075铝合金力学性能的影响 |
| 高川, 邓运来, 王冯权, 郭晓斌 |
|
Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy |
| GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin |
| 图11 强化模型计算结果 |
| Fig.11 Yield strength model calculation results (σp—precipitation strength, σd—dislocation strength, σss—solution strength, σgb—grain boundary strength) (a) total strength prediction (b) precipitation strengthening and dislocation strengthening error |
|