蠕变时效对欠时效7075铝合金力学性能的影响 |
| 高川, 邓运来, 王冯权, 郭晓斌 |
|
Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy |
| GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin |
| 图9 不同时效处理下沿[011]的7075铝合金TEM明场像以及对应的SAED谱 |
| Fig.9 Bright field TEM images and corresponding SAED pattern (inset) along [011] of 7075 aluminum alloy under different aging treatments (a) UA + CA/260 MPa-2 h (b) UA + CA/260 MPa-6 h (c) UA + CA/260 MPa-10 h (d) UA + AA/8 h |
|