蠕变时效对欠时效7075铝合金力学性能的影响 |
| 高川, 邓运来, 王冯权, 郭晓斌 |
|
Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy |
| GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin |
| 图8 不同时效处理的样品EBSD反极图及对应的Taylor因子图 |
| Fig.8 EBSD inverse pole figures (a-d) and corresponding Taylor factor diagrams (e-f) of samples under different aging treatments (a, e) UA + CA/260 MPa-2 h (b, f) UA + CA/260 MPa-6 h (c, g) UA + CA/260 MPa-10 h (d, h) UA + AA/8 h |
|