蠕变时效对欠时效7075铝合金力学性能的影响 |
| 高川, 邓运来, 王冯权, 郭晓斌 |
|
Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy |
| GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin |
| 图2 7075铝合金蠕变试样 |
| Fig.2 7075 aluminum alloy creep specimen (RD—rolling direction, ND—normal direction, TD—transverse direction) (a) sampling position of creep specimen (b) dimensions of creep specimen, tensile specimen, and sampling position of subsequent experiment (unit: mm) |
|