蠕变时效对欠时效7075铝合金力学性能的影响 |
| 高川, 邓运来, 王冯权, 郭晓斌 |
|
Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy |
| GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin |
| 图1 材料制备与析出行为演变过程 |
| Fig.1 Evolution of material preparation and precipitation behavior (SSSS—supersaturated solid solution) |
|