纳米金属层状材料强塑性的界面调控 |
| 郑士建, 闫哲, 孔祥飞, 张瑞丰 |
|
Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites |
| ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng |
| 图15 包含原子台阶的K-S Cu{111}//{110}Nb界面模型[ |
| Fig.15 Side views of K-S Cu{111}//{110}Nb interface models with the atomic steps[ (a) flat interface (b) interface with terrace inside Cu consisting of two Cu{111}//{110}Nb facets on each side (c) interface with terrace inside Cu consisting of one Cu{001}//{110}Nb facet (left) and one Cu{111}//{110}Nb facet (right) (d) interface with terrace inside Nb consisting of two Cu{111}//{110}Nb facets on each side (e) interface with terrace inside Nb consisting of one Cu{001}//{110}Nb facet (left) and one Cu{111}//{110}Nb facet (right) |
|