变形速率对GH3625合金弹-塑性变形行为的影响 |
| 高钰璧, 丁雨田, 李海峰, 董洪标, 张瑞尧, 李军, 罗全顺 |
|
Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy |
| GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun |
| 图8 GH3625合金在0.5 mm/min变形速率压缩变形后组织的TEM像 |
| Fig.8 TEM images showing the microstructures of GH3625 alloy after compression deformation at r = 0.5 mm/min (a) dislocation network(b) dislocation tangle(c) grain (Inset in Fig.8c shows the SAED pattern of deformation band ) |
|