变形速率对GH3625合金弹-塑性变形行为的影响 |
| 高钰璧, 丁雨田, 李海峰, 董洪标, 张瑞尧, 李军, 罗全顺 |
|
Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy |
| GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun |
| 图6 不同状态下GH3625合金的微观组织及其应变分布特征演变 |
| Fig.6 Evolutions of microstructure and strain distribution characteristics in GH3625 alloy under different states (TD—transverse direction, LD—longitudinal direction, TBs—twin boundaries; gray lines show the low angle grain boundaries (LAGBs), black lines show the high angle grain boundaries (HAGBs); Insets show the kernel average misorientation (KAM) images of rectangle regions) (a) solution state (b) r = 0.2 mm/min (c) r = 0.5 mm/min (d) r = 1.0 mm/min |
|