不同服役条件下FGH96合金的蠕变特征
彭子超, 刘培元, 王旭青, 罗学军, 刘健, 邹金文

Creep Behavior of FGH96 Superalloy at Different Service Conditions
PENG Zichao, LIU Peiyuan, WANG Xuqing, LUO Xuejun, LIU Jian, ZOU Jinwen
图3 FGH96合金蠕变曲线
Fig.3 The creep curves of FGH96 superalloy tested at 704oC, 690-810 MPa (a) and 690 MPa, 650-750oC (b)