高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能 |
||||||||||||||||||
| 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟 | ||||||||||||||||||
|
Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact |
||||||||||||||||||
| CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng | ||||||||||||||||||
| 表2 应变速率为700和1600 s-1时原始试样与预压缩试样沿ND冲击的应变速率敏感指数 |
||||||||||||||||||
| Table 2 Strain rate sensitivity indexs of the as-received and precompressed AZ31 magnesium alloy specimen impacted along ND under different true strains (ε) at |
||||||||||||||||||
|
||||||||||||||||||