高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能 |
| 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟 |
|
Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact |
| CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng |
| 图8 预压缩轧制态AZ31镁合金试样和经不同应变速率冲击试样内母晶粒中的孪晶数量分布图 |
| Fig.8 Number of tensile twins in precompressed rolled AZ31 magnesium alloy specimen (a) and impacted along ND under 700 s-1 (b), 1000 s-1 (c), 1300 s-1 (d), and 1600 s-1 (e) |
|