高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能 |
| 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟 |
|
Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact |
| CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng |
| 图11 退孪生晶粒取向变化示意图 |
| Fig.11 Schematics showing the change of orientation during detwinning (a) initial orientation (b) after precompression along RD (c) after impaction along ND |
|