高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能 |
| 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟 |
|
Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact |
| CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng |
| 图5 预压缩轧制态AZ31镁合金沿ND冲击应变速率为1000 s-1时的反极图、晶界图、晶粒尺寸分布图、{0001}极图和取向差角分布图 |
| Fig.5 EBSD analysis results of the precompressed rolled AZ31 magnesium alloy impacted along ND under the strain rate of 1000 s-1 (a) inverse pole figure (b) grain boundary figure (c) grain size distribution (d) {0001} pole figure (e) misorientation angle distribution |
|