高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能 |
| 陈扬, 毛萍莉, 刘正, 王志, 曹耕晟 |
|
Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact |
| CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng |
| 图3 图2a中矩形区域局部放大图及沿图3a中箭头方向的取向差角分布图 |
| Fig.3 Local enlarged figure of the rectangular region in Fig.2a (a) and misorientation angle distribution along the direction indicated by the arrow in Fig.3a (b) |
|