3Mn-0.2C中锰钢形变诱导铁素体动态相变机理 |
| 孙毅, 郑沁园, 胡宝佳, 王平, 郑成武, 李殿中 |
|
Mechanism of Dynamic Strain-Induced Ferrite Transformation in a 3Mn-0.2C Medium Mn Steel |
| SUN Yi, ZHENG Qinyuan, HU Baojia, WANG Ping, ZHENG Chengwu, LI Dianzhong |
| 图7 3Mn-0.2C MMS在T = 660℃、 |
| Fig.7 SEM images and the distributions of Mn of the 3Mn-0.2C MMS deformed to ε = 0.92 under T = 660oC and |
|