3Mn-0.2C中锰钢形变诱导铁素体动态相变机理 |
| 孙毅, 郑沁园, 胡宝佳, 王平, 郑成武, 李殿中 |
|
Mechanism of Dynamic Strain-Induced Ferrite Transformation in a 3Mn-0.2C Medium Mn Steel |
| SUN Yi, ZHENG Qinyuan, HU Baojia, WANG Ping, ZHENG Chengwu, LI Dianzhong |
| 图4 3Mn-0.2C MMS在T = 660℃、 |
| Fig.4 EBSD images of the 3Mn-0.2C MMS at ε = 0.22 (a), 0.51 (b), and 0.92 (c) with the hot deformation under T = 660oC and |
|