3Mn-0.2C中锰钢形变诱导铁素体动态相变机理 |
| 孙毅, 郑沁园, 胡宝佳, 王平, 郑成武, 李殿中 |
|
Mechanism of Dynamic Strain-Induced Ferrite Transformation in a 3Mn-0.2C Medium Mn Steel |
| SUN Yi, ZHENG Qinyuan, HU Baojia, WANG Ping, ZHENG Chengwu, LI Dianzhong |
| 图3 3Mn-0.2C MMS在T = 660℃保温1800 s后和相同温度下以应变速率 |
| Fig.3 SEM images of 3Mn-0.2C MMS soaking at T = 660oC for 1800 s (a) and deformed to ε = 0.51 with |
|