稀土Ce对薄带连铸无取向6.5%Si钢组织、高温拉伸性能和断裂模式的影响 |
| 李民, 李昊泽, 王继杰, 马颖澈, 刘奎 |
|
Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel |
| LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui |
| 图12 CS1和CS2铸带700、800和900℃拉伸断口纵剖面的OM像 |
| Fig.12 Longitudinal OM images of the CS1 (a, c, e) and CS2 (b, d, f) as-cast strips fractured at 700oC (a, b), 800oC (c, d), and 900oC (e, f) |
|