稀土Ce对薄带连铸无取向6.5%Si钢组织、高温拉伸性能和断裂模式的影响 |
| 李民, 李昊泽, 王继杰, 马颖澈, 刘奎 |
|
Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel |
| LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui |
| 图6 CS1和CS2铸带的TEM暗场像及对应的[001]晶带轴选区电子衍射(SAED)花样 |
| Fig.6 Dark field TEM images and the corresponding [001] SAED patterns (insets) of the CS1 (a, c, e) and CS2 (b, d, f) as-cast strips tensile tested at 400oC (a, b), 650oC (c, d), and 800oC (e, f) (APB—antiphase boundary) |
|