添加Ti对Fe22Cr5Al3Mo合金在500℃过热蒸汽中腐蚀行为的影响 |
| 孙蓉蓉, 姚美意, 林晓冬, 张文怀, 仇云龙, 胡丽娟, 谢耀平, 杨健, 董建新, 成国光 |
|
Effect of Ti on the Corrosion Behavior of Fe22Cr5Al3Mo Alloy in 500oC Superheated Steam |
| SUN Rongrong, YAO Meiyi, LIN Xiaodong, ZHANG Wenhuai, QIU Yunlong, HU Lijuan, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang |
| 图7 0.5Ti合金在500℃、10.3 MPa过热蒸汽中腐蚀1000 h时氧化膜截面的HAADF像和EDS面扫描图 |
| Fig.7 HAADF image and EDS mappings of cross-sectional oxide film formed on 0.5Ti alloy corroded in 500oC and 10.3 MPa superheated steam for 1000 h |
|