添加Ti对Fe22Cr5Al3Mo合金在500℃过热蒸汽中腐蚀行为的影响 |
孙蓉蓉, 姚美意, 林晓冬, 张文怀, 仇云龙, 胡丽娟, 谢耀平, 杨健, 董建新, 成国光 |
Effect of Ti on the Corrosion Behavior of Fe22Cr5Al3Mo Alloy in 500oC Superheated Steam |
SUN Rongrong, YAO Meiyi, LIN Xiaodong, ZHANG Wenhuai, QIU Yunlong, HU Lijuan, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang |
图5 0Ti、0.5Ti和1.0Ti合金在500℃、10.3 MPa过热蒸汽中腐蚀3、500和1000 h的氧化膜表面显微组织SEM像 |
Fig.5 SEM images of surface morphologies of oxide films formed on 0Ti (a1[24]-a3), 0.5Ti (b1-b3), and 1.0Ti (c1-c3) alloys corroded in 500oC and 10.3 MPa superheated steam for 3 h (a1[24]-c1), 500 h (a2-c2), and 1000 h (a3-c3) |
![]() |