三维石墨烯/Cu复合材料在模拟海水环境中的腐蚀和空蚀行为 |
| 潘成成, 张翔, 杨帆, 夏大海, 何春年, 胡文彬 |
|
Corrosion and Cavitation Erosion Behavior of GLNN/Cu Composite in Simulated Seawater |
| PAN Chengcheng, ZHANG Xiang, YANG Fan, XIA Dahai, HE Chunnian, HU Wenbin |
| 图7 Cu及3D-GLNN/Cu复合材料在NaCl中浸泡1 h后的Bode图(欧姆电阻校正后) |
| Fig.7 Ohm resistance-corrected Bode plot for Cu and 3D-GLNN/Cu composites after immersing in NaCl solution for 1 h |
|