脉冲电流调控金属固体中的残余应力 |
| 张新房, 向思奇, 易坤, 郭敬东 |
|
Controlling the Residual Stress in Metallic Solids by Pulsed Electric Current |
| ZHANG Xinfang, XIANG Siqi, YI Kun, GUO Jingdong |
| 图4 高能脉冲电流多参数(电容充电电压)处理下材料x方向和y方向残余应力随处理时间演化关系[ |
| Fig.4 Evolution relationship of residual stresses in x direction (σx ) |
|