脉冲电流调控金属固体中的残余应力 |
| 张新房, 向思奇, 易坤, 郭敬东 |
|
Controlling the Residual Stress in Metallic Solids by Pulsed Electric Current |
| ZHANG Xinfang, XIANG Siqi, YI Kun, GUO Jingdong |
| 图1 残余应力在不同尺度的分类[ |
| Fig.1 Residual stress classification at different scales[ |
|