基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究
丁宗业, 胡侨丹, 卢温泉, 李建国

In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology
DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo
图12 氢气泡尺寸增加发生跳跃行为和化合物溶解导致氢气泡发生跳跃行为的示意图
Fig.12 Schematics of hydrogen bubbles jumping with the increasing volume (a) and hydrogen bubbles jumping due to the IMCs dissolution (b) (F—force on the bubble; R1, R2—radii of the two ends of the deformed bubble)