基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究 |
| 丁宗业, 胡侨丹, 卢温泉, 李建国 |
|
In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology |
| DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo |
| 图11 Al/Ni液/固界面第一阶段变形氢气泡迁移合并的实时成像,第二阶段静止吞并行为的实时成像和示意图,及Al/Ni液/固界面氢气泡的合并行为的实时成像 |
| Fig.11 In situ images of migration and coalescence of hydrogen bubbles during the first stage at the liquid Al/solid Ni interface (a), in situ images and schematic diagram of annexation of static hydrogen bubbles during the second stage at the liquid Al/solid Ni interface (b), and in situ images of coalescence of hydrogen bubbles at the liquid Al/solid Ni interface (c, d) ( J1 and J3 represents the H diffusion fluxes through the bubble/melt interface of large bubble and small bubble, respectively; J2 indicates the H diffusion flux between different bubbles with various radius; |
|