基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究 |
| 丁宗业, 胡侨丹, 卢温泉, 李建国 |
|
In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology |
| DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo |
| 图10 Al/Ni液/固界面中Al枝晶和金属间化合物为凹槽衬底的氢气泡异质形核示意图 |
| Fig.10 Schematics of heterogeneous nucleation of hydrogen bubbles on the concave Al dendrites (a) and concave IMCs (b) at the liquid Al/solid Ni interface |
|