基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究 |
| 丁宗业, 胡侨丹, 卢温泉, 李建国 |
|
In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology |
| DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo |
| 图5 Al/Ni液/固界面加热过程中Al3Ni金属间化合物溶解与氢气泡生长的实时成像 |
| Fig.5 In situ images of Al3Ni intermetallic compounds (IMCs) dissolution and bubbles growth during heating at the liquid Al/solid Ni interface (a) 596℃, 201 s (b) 607℃, 211 s (c) 612℃, 216 s (d) 621℃, 225 s (e) 631℃, 235 s (f) 634℃, 237 s (g) 646℃, 245 s (h) 660℃, 251 s (i) 678℃, 260 s (j) 685℃, 264 s (k) 692℃, 269 s (l) 693℃, 270 s (m) 695℃, 271 s (n) 718℃, 281 s (o) 750℃, 348 s |
|