基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究 |
| 丁宗业, 胡侨丹, 卢温泉, 李建国 |
|
In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology |
| DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo |
| 图3 氢气泡数量随时间的变化,群体气泡平均尺寸随时间的变化,阶段1及阶段2不同区域气泡的平均尺寸变化 |
| Fig.3 Relationship between hydrogen bubbles number and heating time (a), mean diameter of groups of hydrogen bubbles versus heating time (b), mean diameter of the groups of hydrogen bubbles in the different regions during the first stage (c) and the second stage (d) (R2 indicates mean squared error. The different colored lines in Fig.3d represent different bubbles during the second stage) |
|