基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究 |
| 丁宗业, 胡侨丹, 卢温泉, 李建国 |
|
In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology |
| DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo |
| 图2 Al/Ni液/固界面加热过程中非均匀熔体不同区域氢气泡的实时生长放大图 |
| Fig.2 Magnifications of real-time images of hydrogen bubbles growth in region II (a), region III (b), and region IV (c) of inhomogeneous melts during heating at the liquid Al/solid Ni interface |
|