汽车用先进高强度冷轧双相钢的显微组织调控和强韧化机理 |
| 储双杰, 毛博, 胡广魁 |
|
Microstructure Control and Strengthening Mechanism of High Strength Cold Rolled Dual Phase Steels for Automobile Applications |
| CHU Shuangjie, MAO Bo, HU Guangkui |
| 图5 两相区退火工艺参数对双相钢的显微组织演变的影响[ (a) intercritical annealing temperature (b) intercritical annealing time (c) heating time |
| Fig.5 Effects of intercritical annealing parameters on the microstructure evolution of dual phase steels (vh—heating rate, T—annealing temperature, t—holding time, vc—cooling rate, MLI—mean linear intercept)[ |
|