核级镍基合金焊接材料失塑裂纹研究现状 |
| 余春, 徐济进, 魏啸, 陆皓 |
|
Research Status of Ductility-Dip Crack Occurring in Nuclear Nickel-Based Welding Materials |
| YU Chun, XU Jijin, WEI Xiao, LU Hao |
| 图2 Inconel 52M焊缝金属的OM像及其大角度晶界上析出相的SEM像[ |
| Fig.2 OM image of Inconel 52M weld metal (a) and SEM image of precipitates at high-angle grain boundary (b)[ |
|