图6 NiCoCrAlFe高熵合金粉体氧化之后的截面形貌与元素分布[55]
(a, b) low magnification and locally amplifying BSE images after 48 h oxidation at 900oC (c, d) low magnification and locally amplifying BSE images after 48 h oxidation at 1000oC (e, f) low magnification and locally amplifying BSE images after 48 h oxidation at 1100oC
Fig.6 Cross-sectional morphologies and elemental maps of NiCoCrAlFe HEA powder after oxidation[55]