激光熔覆高强韧铁基涂层精细组织调控与性能研究 |
| 冯凯, 郭彦兵, 冯育磊, 姚成武, 朱彦彦, 张群莉, 李铸国 |
|
Microstructure Controlling and Properties of Laser Cladded High Strength and High Toughness Fe-Based Coatings |
| FENG Kai, GUO Yanbing, FENG Yulei, YAO Chengwu, ZHU Yanyan, ZHANG Qunli, LI Zhuguo |
| 图18 熔覆层中不同深度的XRD分析[ |
| Fig.18 XRD analyses of the coating at different distances from the interface of coating/substrate[ (a) SEM image of coatings (b) XRD spectra at different depths (c) fusion line between coating and substrate |
|